TL;DR "hydrofluoric acid is a water solution of hydrogen fluoride, HF. That’s a gas, and it’s a lot worse. ... As soon as it hits anything moist – like your lungs – it dissolves in the water and turns into hydrofluoric acid again."
[ Parent
| on HN ]
Re:A home-made lithographically-fabricated integrated circuit
by lifeisstillgood on Monday April 30, 2018 @03:53AM
(#16956637)
or
"The straight liquid must really be a treat, but I’ve never seen it in that form, and would only wish to through binoculars."
Re:A home-made lithographically-fabricated integrated circuit
by AstralStorm on Monday April 30, 2018 @04:05AM
(#16956686)
The fact that it is liquid at relatively balmy temperatures makes it a bit easier to handle than most gases, but then you better have great urethane seals, gloves and clothing everywhere. (Silicones are permeable, PTFE is damaged over time, nitrile and vinyl gloves also leak.)
Re:A home-made lithographically-fabricated integrated circuit
by jakeogh on Monday April 30, 2018 @05:38AM
(#16957120)
8mil nitrile x2 with no extended(!) contact option. Like silane: http://amo-csd.lbl.gov/downloads/Chemical%20Resistance%20of%...