News for hackers. Stuff that matters.
Re:Fifty or Sixty Years of Processor Development for This? by Tuna-Fish on Wednesday April 04, 2018 @07:55AM (#16753854)
In the biz people already measure some widths as "monolayers", which refers to a single layer of atoms. Some process features have error margins of less than a monolayer -- that is, a dieletric needs to be 4 monolayers thick, and if it only has 3, the device is going to short, and if it has 5, the device will not work.
Re:Fifty or Sixty Years of Processor Development for This? by jjoonathan on Wednesday April 04, 2018 @09:34AM (#16754499)
What kind of CVD/PVD process do you use to achieve those kinds of tolerances? Or is the trick to use protect/deprotect steps like in conventional chemistry?
Re:Fifty or Sixty Years of Processor Development for This? by deepnotderp on Wednesday April 04, 2018 @12:25PM (#16756257)
ALD is commonly used for these ultra fine tolerances.