I remember watching a teardown of a spare-no-expense embedded military computer, and the guy couldn't stop talking about how much "conformal coating" the board had.
Edit: I think this is the video: https://www.youtube.com/watch?v=55z_0BYb5is
It is not used for Sn (tin) whiskers at all, since it wouldn't penetrate the pads/package of the IC and wouldn't stop such a high modulus process in any case. Whiskers are most problematic with modern Pb-free solders and fine pitch SMT practices (QFNs & BGAs), but it's worth noting that other materials (like Zn) also have significant issues.
> The coating completely penetrates spaces as narrow 0.01mm.
I would have thought that would make it very effective in protecting against whiskers in QFPs that might have a lead pitch of 0.4mm or larger. There's not a lot you can do under the bodies of BGAs and QFNs, but if you're worried about whiskers you're probably using QFPs instead.
This app note suggests that Parylene and a few other dip-type conformal coatings do slow down tin whiskers, but don't stop their spread:
https://www.maximintegrated.com/en/app-notes/index.mvp/id/52...
Here is Mike's BBC micro : https://www.youtube.com/watch?v=la-sGpTpkxE
Great stuff.
Tl;dr: Tin whiskers are very thin spontaneous metallic formations which can short nearby pcb tracks or conductors and are believed to be the cause of many failures in electronic devices. There is no evidence of a single cause for their formation but it seems certain that eliminating lead (RoHS legislations etc.) from solder is one of them.