Re:What Kind of Lithography Will Be Used at 7nm? by asmithmd1 on Wednesday March 09, 2016 @07:39PM (#11256698)
At 7nm spacing you could draw 100,000 lines across the width of a human hair. About 70 silicon atoms lying next to each other would be 7nm wide. I know the end of Moore's law has been predicted before, but this time has to be different.
Re:What Kind of Lithography Will Be Used at 7nm? by nhaehnle on Wednesday March 09, 2016 @09:28PM (#11257096)
Keep in mind that most features at 7nm would be quite a bit larger than 7nm. For example, in the 22nm technology I have worked with, a standard wire on the lowest metal layer might be around 40nm wide (higher metal layers use even wider wires to benefit from their lower resistance to cross larger distances).

I do agree with your fundamental point that there will definitely be an end to Moore's law. It's just that the mere number of silicon atoms doesn't make <7nm infeasible.

Re:What Kind of Lithography Will Be Used at 7nm? by esmi on Thursday March 10, 2016 @03:40AM (#11257974)
28nm was the last node in Moore's law. Transistors are smaller, but not cheaper. http://www.eetimes.com/author.asp?doc_id=1321536

I should also add, many people think 5nm will be technically feasible, although I don't think anyone knows how at scale, but there are serious question as to whether or not it makes economic sense. Thus the node may not be developed for some time, but because of business reasons.

Re:What Kind of Lithography Will Be Used at 7nm? by hga on Thursday March 10, 2016 @05:10AM (#11258265)
That article is very interesting, it says what sounds like fundamental SRAM (cache) scaling limits being hit is a if not the major factor, so the prospect of EUV decreasing the number of masks required won't help as much as I thought it might in decreasing costs. And as noted in the OP, EUV still have to prove itself in power and uptime.
Re:What Kind of Lithography Will Be Used at 7nm? by userbinator on Wednesday March 09, 2016 @10:21PM (#11257231)
Is it like how inkjet printers advertise huge resolutions like 5760dpi, and the positioning can achieve that resolution, but the actual nozzles can't produce lines thinner than e.g. 720dpi?
Re:What Kind of Lithography Will Be Used at 7nm? by ghaff on Wednesday March 09, 2016 @10:32PM (#11257255)
No. There are process nodes that have real technical meaning but, especially as sizes shrink, what that means exactly in terms of the dimensions of specific features varies considerably.
Re:What Kind of Lithography Will Be Used at 7nm? by avian on Thursday March 10, 2016 @07:36AM (#11258797)
The "Minimum feature size" slide included in this article shows some feature sizes for existing technologies. I think names like "14 nm" and "7 nm" are mostly marketing at this point.

http://www.anandtech.com/show/8367/intels-14nm-technology-in...

Re:What Kind of Lithography Will Be Used at 7nm? by b1661727 on Thursday March 10, 2016 @08:25AM (#11258998)
Each dot can only have a single color. Multiple dots will form a single "pixel" with the desired color.
Re:What Kind of Lithography Will Be Used at 7nm? by 13of40 on Wednesday March 09, 2016 @10:34PM (#11257259)
I think it's more like Elmo's head is four inches wide on the screen but the pixels are two millimeters.
Re:What Kind of Lithography Will Be Used at 7nm? by mrob on Thursday March 10, 2016 @09:02AM (#11259202)
That's better than pure 720dpi. In GIMP, try using the Erode filter on ultra-light weight fonts. Although the minimum feature size is increased you still get the benefit of smoother curves. It looks better than a normal weight font that's been scaled up from low resolution.